CARACTERISATION DE MATERIAUX BICOUCHES PAR ULTRASONS LASER : MODELISATION SEMI-ANALYTIQUE ET VALIDATION EXPERIMENTALE
R. Coulette 1,2 , E. Lafond 3 , M.-H. Nadal 1 , C. Gondard 1 , C. Grand 4 , F. Lepoutre 2 et O. Pétillon 3 ( 1 CEA/DAM - IS-SUR-TILLE - France, 2 ONERA - CHATILLON - France, 3 AEROSPATIALE - SURESNES - France - 4 LOA - PARIS - France)