APPLICATION DE LA MÉTHODE IMPACT ECHO POUR LA DETECTION DE VIDES OU LA RECHERCHE D'EPAISSEURS DANS LE BETON
O. ABRAHAM*, J. ALEXANDRE*, M. KAHAN** *LCPC - BOUGUENAIS - France / **SETRA - BAGNEUX - France

Source:
Abstracts of the 1997 COFREND Congress on Nondestructive Testing, September 22-26, 1997 - Nantes France.