APPLICATION DE LA TOMOGRAPHIE X A LA MESURE DE DENSITE DES ACIERS FRITTES
P. Franco* - F. Roy** - C. Delarche** *CEA/Le Ripault, MONTS (France) - **PSA, VELIZY (France)

Source:
Abstracts of the 1997 COFREND Congress on Nondestructive Testing, September 22-26, 1997 - Nantes France.