UTILISATION DES ONDES DE LAMB POUR DETECTER DES DEFAUTS DANS DES MATERIAUX COMPOSITES
C. Potel 1,2 , S. Baly 1 , J.F. de Belleval 1 , O. Pétillon 3 , J.L. Arnaud 3 1 Univ. Tech. Compiègne, LG2mS, UPRES ass. CNRS, COMPIEGNE, France 2 Univ. Picardie Jules Verne, IUT d'Amiens, Dépt. OGP SOISSONS, France 3 Aérospatiale, Centre Commun de Recherches L. Blériot, SURESNES, France

Source:
Abstracts of the 1997 COFREND Congress on Nondestructive Testing, September 22-26, 1997 - Nantes France.