CONTROLE NON DESTRUCTIF DE LA MASSE VOLUMIQUE DES COUCHES DE CHAUSSEES
M.L. Gallenne, M. Davy, J. Godin, G. Morel (LCPC / CCA / LRPC / CER - NANTES / ANGERS / ROUEN -France)

Source:
Abstracts of the 1997 COFREND Congress on Nondestructive Testing, September 22-26, 1997 - Nantes France.