Record cntrl number :199411173
Quality valid. date :1994-11-25
Title in english :STUDY OF A PROCEDURE FOR THE INSPECTION OF STRUCTURAL
COMPONENTS MADE OF ANISOTROPIC COMPOSITE MATERIALS WITH POLYMETRIC
MATRIX
Author :ORILIO I
DENIS R
LAKESTANI F
Affiliation :CIRA, CAPUA (IT)
CIRA, CAPUA (IT)
CIRA, CAPUA (IT)
Bibliogr reference :PAPER PRESENTED: 6TH EUROPEAN CONFERENCE ON
NON-DESTRUCTIVE TESTING, NICE (FR), OCTOBER 24-28, 1994 AVAILABLE
FROM EUROPEAN COMMISSION, DGXIII/D-2, L-2920 LUXEMBOURG AS PAPER EN
38534 ORA
Abstract :This article studies the non-destructive techniques
employed for the inspection of anisotropic composite materials. A
good knowledge of the anisotropic properties of the carbon fibre
composite is required for the prediction of the ultrasonic response
from known reflectors and for the interpretation of the inspection
results. The elastic constants and the attenuation factors were
measured and, successively, experimental echodynamic curves on 30 ,
45 and 60 slots were successfully compared with theoretical
predictions.
Facet codes :608 Materials testing and derived properties
Availability in lang :en
Publication year :1994
Publication type :ORA
Euroabstracts number :EAB132149200
Programme acronym :ADVMAT 2C
Commission service :JRC
Subject index codes :MAT (MATERIALS TECHNOLOGY)
Rolf Diederichs 1. Sept 1996,