Record cntrl number   :199311281
Quality valid. date   :1994-11-29
Title in english      :ULTRASONIC NON-DESTRUCTIVE TESTING OF IMPACT DAMAGE
       IN COMPOSITE MATERIALS
Original title        :ISPEZIONE NON DISTRUTTIVA ULTRASONORA DEL
       DANNEGGIAMENTO     DA     IMPATTO     NEI     MATERIALI     COMPOSITI
Author                :PEZZONI R
       MERLETTI L
       BATTAGIN G
       DENIS R
Affiliation           :LABORATORIO TECNOLOGIE SPERIMENTALI - AGUSTA (IT)
       LABORATORIO TECNOLOGIE SPERIMENTALI - AGUSTA (IT)
       JRC ISPRA (IT)
       JRC ISPRA (IT)
Bibliogr reference    :PAPER PRESENTED: XII CONGRESSO NAZIONALE AIDAA, COMO
       (IT), JULY 20-23, 1993 AVAILABLE FROM EUROPEAN COMMISSION, DGXIII/D-2
        L-2920      LUXEMBOURG      AS      PAPER      IT      37820     ORA
Abstract              :This report describes the techniques and methods used
       to  perform  ultrasonic non-destructive tests on samples of composite
       structures  with  a  thermosetting  epoxy  matrix and carbon or glass
       fibre, in both laminated and sandwiched form. A description is given,
       for  each  sample,  of  the  methods  used to build a high resolution
       ultrasound image to show the actual extent of the damaged area.
       Experimental  results  are  given  and  the equipment and calibration
       methods  needed  to ensure the correct capture of ultrasonic data are
       described.  Reference  is  also  made  to  the  application  of these
       techniques  to  both  samples  and  actual  assemblies  during  civil
       certification  tests  for  components  of  the  Agusta-Westland EH101
       helicopter.
Facet codes           :605 Composite materials
Availability in lang  :it
Publication year      :1993
Publication type      :ORA
Euroabstracts number  :EAB131189700
Commission service    :JRC
Subject index codes   :MAT (MATERIALS TECHNOLOGY)

Source: Cordis http://www.cordis.lu
Cordis Copyright Information

| Front Page | | Abstract list|

Rolf Diederichs 1. Sept 1996, info@ndt.net