On the basis of these estimations, we have judged that it would be judicious to encourage the automatic ultrasonic testing. For this purpose and in the goal to approach the ultrasonic testing method by the radiography on adopting the imagery and the signal processing to the ultrasonic techniques, we present the < References:
Fig.
1. J.L.Pelletier, La pratique du controle industrielpar ultrasons, tome2, edition ENSAM 84
2. Radiographs of welds, iis 91
3. F.Bettayeb, B.Maamache, S.Debbache, Syso: systeme expert d 'aide au diagnostic descauses des defauts de soudage a I 'arc, in proceeding COM'CND, Algiers 28-30 June 97
Abstract Source: