Optimization of Cd1-xZnxTe Detectors for Digital Radiography

G. C. GIAKOS, B. PILLAI, S. VEDANTHAM, S. CHOWDHURI, A. DASGUPTA, R. B. RICHARDSON, P. GHOTRA, R. J. ENDORF, A. PASSALAQUA, AND W. J. DAVROS
ABSTRACT
start  previousnext

Publication Source: Journal of X-Ray Science and Technology, ISSN: 0895-3996. Volume 8, Number 2, 1998. Pages: 37...