M. G. Horsten, ECN, Petten, The Netherlands; P. Kauppinen, VTT, Espoo, Finland; M. Kröning, IZFP, Saarbrücken, Germany, J. Bros, Tecnatom, Madrid, Spain; M. Hutchings, AEA Technology, Cheshire, U.K.; D. Gomez Briceno, CIEMAT, Madrid, Spain; H. Weimann, ARCS, Seibersdorf, Austria
Furthermore, it would make it possible to assess on field various components that now-a-day can only be assessed either by calculation or by means of very expensive sample gaining techniques. This last factor would mean a terrific increase in EC citizen safety.
About the feasibility, it has to be noted that a growing numbers of publication on the subject are appearing more and more in the proceedings of International Conferences like the recent ICONE Conference.
This AMES-NDT Concerted Action is aiming to undertake the intermediate needed step of listing all known techniques, their application and limits and the report on sample demonstration tests before a proper systematic qualification of techniques.
![]() | Materials Properties Measurement | ![]() |