Artificial Intelligence as an Instrumentation for a Comprehensive Analysis of Concrete Curing by Ultrasonic Method

Edouard G. Nesvijski, Alexandre Lorrenzi, Odilon P. Cavalheiro, and Marco A. Pozzobon UFSM, Centro de Tecnologia, Santa Maria, RS, Brasil