| INSPEC Antwortnummer 8 - © 1998 IEE |
| Title |
| | Love wave propagation in a solid with a cold-worked surface layer. |
| Author |
| | Hirao, M.; Sotani, Y. (Faculty of Engng. Sci., Osaka Univ., Toyonaka, Osaka, Japan); Takami, K.; Fukuoka, H. |
| Publication Source |
| | Journal of Nondestructive Evaluation (March 1981) vol.2, no.1, p.51-5. 3 refs. CODEN: JNOED5 ISSN: 0195-9298 |
| Document Type |
| | Journal |
| Treatment Code |
| | Theoretical; Experimental |
| Country of Publication |
| | United States |
| Language |
| | English |
| Abstract |
| | Experiments show Love wave generation along the top surface of used railroad rail, where the shear wave velocity has been slightly reduced by the cold-working of wheel passage for years. The RF pulses used in the experiments have about 10 mu s duration and a relatively narrow frequency spectrum. The group velocity of the Love wave is found to have a strong dependence on the carrier frequency over the tested range of 0.45-3.1 MHz. Application of the seismological one-layered model to the experimental measurements yields an NDE technique for the elastic properties and the thickness of the cold-worked surface layer. The results are interpreted on the basis of a destructive observation by micro-Vickers hardness testing. |
| Accession Number |
| | 82:1872362 |