| Abstract | |
| A system for the examination of the structural integrity of railway wheels in motion using both ultrasonic Rayleigh surface waves and sonic excitation is presented. While certain technical aspects of this project have reached an advanced state of development overseas, the over-all automation and computerization and the statistical interpretation of the results are being developed in Australia.-AA | |
| Accession Number | |
81(9):22-1196 | |
| |NDTnet| |Abstract Database| |Railway Abstracts| |