| Title |
| | Non-Destructive Testing on the Southern Railway System. |
| Author |
| | Rohr, T.C. |
| Publication Source |
| | ASNT National Fall Conf., Denver, Colorado, Oct. 1978 (1978), 397 |
| Document Type |
| | Journal |
| Language |
| | English |
| Abstract |
| | See Met.A., 7912-72 0438. A brief account is given of the components of a U.S. railroad which are amenable to non-destructive testing, i.e. the rails and the railroad cars. Track geometry is measured by a special car. Flanged wheels cannot yet be reliably tested. -M.J. |