| Title | |
| Overview of Current Efforts to Detect and Prevent Steel Wheel Failures. | |
| Author | |
| Leadley, Gary L. | |
| Publication Source | |
| Detection, Diagnosis and Prognosis. NBS Spec. Pub. No. 436, U.S. Dept. of Commerce (Available from U.S. Govt. Printing Office, Washington, D.C. 20234). 1975, 261-283. | |