| 4th International Conference of Slovenian Society for NDT Table of Contents | Inservice Inspection Of Pressure Vessels By The B-Scan MethodI. Vojvoctic - Gvardjancid*, J Zorko***Institute of metals and technology, 1000 Ljubljana, Slovenia; **Nuclear power plant Krsko, 8270 Krsko, Slovenia |
Keywords: Ultrasonic TestingInfrastructure, Systems, Operations, Processes, Management, Motivation, Environment,Quality, Competition, Investment, Joint Ventures
Source: Conference Proceedings of the 4th International Conference of the Slovenian Society for Nondestructive Testing, 24 - 25 April 1997, Ljubljana, Slovenia.
Pages:335 - 339