Abstract:
Ultrasonic Testing in Pipe Extrusion
Foreword from the Author
This On-Line guide book is a HTML edition of seminars and publications[References]
from the author Rolf Diederichs.
This hand book should give newcomers to the extrusion market help with decisions,
or making for current user a further knowledge base for this technology.
There are, even for Ultrasonic NDT users, some
useful reading.
The state of the art revued here, relates to [References]
the years 1991 -1992. Some of the guide books´ content were at that time in their early stage
, or just announced. This technology gained during the last years, more
and more industrial standards and it is still today very topical.
Nevertheless the author will, after some other HTML publications,
update this edition.
Copyright is for Internet and other electronic media always
a debatable issue. It is acceptable for readers to make a personal copy
. But for any further copies or commercial use,
the copyright law is relevant.
I welcome your suggestions now here via mail.
©copyright Rolf Diederichs 13. Dec 1995
- Introduction
- Ultrasonic mechanics
Overview, fixed Transducers, Measurement Chamber,...Scanner....
- Measurement position in the Extrusion line
Possibilities, advantages/disadvantages, praxis experiences. with clickmap
- Requirements for the Ultrasonic System
Result display, Operations, Feedback, Protocol, Interfaces
- Coextrusion Layer Thickness Measurement
Wide Range, Example Car Gasoline Pipe
- Ultrasonic Flaw Detection
Definition, Types of Flaws, System Requirement, Evaluation , Test
Mechanics
- Practical Example
An Ultrasonic Measurement System controls precise the Inner and
Outer Diameter of Plastics Pipes at a Netherlands manufacturer
for Irrigation pipes
- Conclusion and Prospects
Appendix
- References
- New advantages for quality control of Plastic Gas Pipes with an
Ultrasonic Flaw Detection Rotation Machine
- Report about the K'95 Plastic fair
- FAQ-Frequent asked questions
With an input form for your question - you will get answer via email.
- Echo Image Examples
The Echo Image Series is a selection of Echo Signals. The series pick up common situations of Echo Signal conditions and display
them with their RF Signal.
- Alphabetically Subject Index
also with an Index of Figures [gifs]
- Tabulation
Plastic Materials and their acoustic properties.