So far creep is concerned there is no nondestructive method to detect it except by the technique called Automatic Ultrasonic Scanning (AUS). By this method, creep effect can be detected even in early stages and hence replacement of a heater tube due to creep development can be planned safely ahead of failure.
The paper deals with the Auto US technique, a very powerful non- destructive technique with emphasis mainly on application details.