EXPERIMENTAL STUDY OF THE VELOCITY EFFECT ON THE MAGNETIC FLUX LEAKAGE TESTING OF THE THIN STEEL STRIP

Zhongsoo Lim, Goohwa Kim, and Derac Son
Research Institute of Industrial Science and Technology
P. O. Box 135, Pohang, Kyungbuk, 790-600, Korea
Physics Department, Hannam University, 133, Ojung Dong, Daejon, 306-010, Korea
ABSTRACT
start  previousFull Paper Not Received next

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.full paper not received