PROBLEMS OF NON-LINEARITIES IN LASER STIMULATED NON-DESTRUCTIVE HEAT TREATMENT OF SURFACE

M. A. Razumova and A. D. Suprun
Department of Physics, Kyiv T. Shevchenko University
prospekt Glushkov 6, 252022, Kyiv, Ukraine
ABSTRACT
start  previousOptical Methodsnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 3, pages 1489 - 1492