GRADING OF SWAN TIMBER - ELASTO SONIC WAY

K. Shyamasundar, B. S. Aswathanarayana and M. Venugopal Naidu
Indian Plywood INdustries Research and Training Institute, P. O. Box 2273, Bangalore 560 022, India
ABSTRACT
start  previousNDE of Compositesnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 2, pages 761 - 764