tb'. The Bauschinger's effect and strain hardening after reverse-yielding are taken into account. The pe of autofrettaged cylinder will be compared with measurements made by the re-yield method and calculation from the
tb' obtained by the X-ray diffraction means. The relative error is within ±10%. ![]() | Full Paper Not Received | ![]() |