EVALUATING THE FATIGUE DAMAGE OF MATERIAL BY USING BARKHAUSEN NOISE METHOD

Li qiang Yuan Zuyi Miao Longxiu
Department of Mechanical Engineering, Northern Jiaotong University, Beijing 100044
ABSTRACT
start  previousMagnetic Techniquesnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 3, pages 1611 - 1614