QUALITY OF SEAL DISCS-THROUGH NDT

S. P. Srivastava, A. Manjunatha, M. Jayandranath
Central Workshops, B. A. R. C., Bombay-85, India
ABSTRACT
start  previousNDE of Defectsnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 2, pages 961 - 966