ADVANCES IN MAGNETIC METHODS FOR WALL THICKNESS MEASUREMENT IN FERROMAGNETIC TUBE AND PLATE

Roderic K. Stanley, Quality Tubing Inc.
Houston, Texas, USA
ABSTRACT
start  previousFull Paper Not Received next

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.full paper not received