DEVELOPMENT OF TEST PROCEDURES AND RESULTS OF HELIUM LEAK TESTING OF Nb-Ti SUPERCONDUCTOR BILLETS

N. G. Dutta, Anis Ahmad, P. G. Kulkarni and D. S. C. Purushotham
Atomic Fuels Division, Bhabha Atomic Research Centre
Trombay, Mumbai 400 085, India
ABSTRACT