EFFECT OF SURFACE ROUGHNESS ON CADMIUM PLATING THICKNESS MEASUREMENT USING MAGNETIC METHODS

M. Arumugam, T. Rethnapandian, G. Raju, N. Girijan and S. Mahadevan
QDMF/SR, Vikram Sarabhai Space Centre, Thiruvananthapuram 695 022, India
ABSTRACT
start  previousMagnetic Techniquesnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 3, pages 1635 - 1638