EVALUATION OF CARBURIZATION DEPTH IN SERVICE EXPOSED FERRITIC STEEL USING MAGNETIC BARKHAUSEN NOISE ANALYSIS

V. Moorthy, S. Vaidyanathan, T. Jayakumar and Baldev Raj
Division for PIE and NDT Development
Indira Gandhi Center for Atomic Research, Kalpakkam 603 102
ABSTRACT
start  previousMagnetic Techniquesnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 3, pages 1639 - 1642