ACOUSTIC EMISSION DURING TENSILE DEFORMATION AND FRACTURE OF A NUCLEAR GRADE AISI TYPE 304 STAINLESS STEEL SPECIMEN WITH NOTCHES

C. K. Mukhopadhyay, T. Jayakumar and Baldev Raj
Metallurgy and Materials Group
Indira Gandhi Centre for Atomic Research, Kalpakkam 603 102, India
ABSTRACT
start  previousAET Fatigue and Fracturenext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 4, pages 2389 - 2392