AN ACOUSTIC-TESTING SENSOR BASED ON ACOUSTO-MAGNETIC EFFECT

Yougen Peng
Department of Metal Material Engineering, North China Institute of Technology
PO BOX 13, Taiyuan, Shanxi 030051, China
ABSTRACT
start  previousUltrasonic Technique - Sensor Technologynext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 4, pages 2019 - 2022