CREEP CRACKING AND ACOUSTIC EMISSIONS IN POLAR SHELF ICE AT HIGH TEMPERATURE OF 0.96 Tm

Nirmal K. Sinha
National Research Council, Building M-17
Ottawa, Ontario, Canada K1A OR6