DYNAMIC INDENTATION METHOD FOR THE ESTIMATION OF MECHANICAL PROPERTIES OF MATERIALS

Valery A. Rudnitsky, Alexander V. Rabtchevich
Institute of Applied Physics of Belarussian Academy of Sciences
16, F. Skoryna Str., Minsk 220072 BELARUS
ABSTRACT
start  previousVibration Monitoringnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 2, pages 1129 - 1132