COMPUTATION OF EXCHANGE INTEGRAL AND QUANTITATIVE INDICATION OF FERROMAGNETISM

Xu Jiazhen, Xu Shufa*, Liu Yueming**
Chongqing Jianzhu University, P. R. China
*Workers & Stuff University of Chongqing Municipal Bureau of Machine Building
**Shenzhen Lingke Limited Company of Telecommunication
ABSTRACT
start  previousMT - Magnetic Techniquesnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 3, pages 1585 - 1588