PREDICTION OF FAILURE BEHAVIOUR IN COMPOSITE PRESSURE VESSELS BY HYDRO PROOF ACOUSTIC EMISSION

Sung-Jin Song, In-Young Yang, Chi-Hwan Oh1, Soo-Yong Lim*, Sang-Ho Rhee*, and Ho-Chul Kim**
Factory Automation Research Center for Parts of Vehicles and Department of Mechanical Design Engineering, Chosun University, Kwangju, 501-759 Korea
*Agency for Defense Development, Taejon, 300-600 Korea
**Department of Physics, Korea Advanced Institute of Science and Technology, Taejon, 305-701, Korea
ABSTRACT
start  previousAET - AET - Pressure Vesselsnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 4, pages 2413 - 2416