CORRELATION OF VARIOUS ELASTIC MODULI WITH RELATIVE DENSITY OF POROUS ALPHA-TWO TITANIUM ALUMINIDE COMPACTS

Theodore E. Matikas, Prasanna Karpur, Robert L. Crane, S. Shamasunder*
USAF Wright Laboratory Materials Directorate (UDRI), WL/MLLP
Wright-Patterson Air Force Base, OH 45433-7817
*USAF Wright Laboratory Materials Directorate (UES, Inc.), WL/MLLN
Wright-Patterson Air Force Base, OH 45433-7817
ABSTRACT
start  previousUT - Ultrasonic Testing - Mechanical Propertiesnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 4, pages 2271 - 2274
Publisher: Ashgate Publishing Company