PENETRANT TEST DEVELOPMENT MECHANISM AND DEVELOPER MOLECULAR STRUCTURE
Lin Zhenwang*, Gong Decheng *, Chen Zhenlu1, He Xiutang** * Xiamen Chemical Machinery Plant, Fujian, China ** Huaqiao University, Quenzhou, Fujian, China
This paper take the common quick drying solvent suspension developer as an example, describe the development adsorption course. Inquire the relative of the different solvent their different surface activity, and the different developer their different molecular structure, different dispersion energy and polarity energy with the develop sensitivity. Discuss the developer power different specific surface area influence the capillarity and sensitivity. Which give a reference for Penetrant Test scientific worker to raise PT sensitivity.
Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 2, pages 1231 - 1234 Publisher:Ashgate Publishing Company