ADVANCED DAMAGE ASSESSMENT OF CREPT POWER PLANT COMPONENTS BY MULTILAYER IN-SITU SECTIONING AND REPLICATION

G. Venkataraman, T. R. Ramesh, R. Veeraragavan and R. S. Babu
Welding Research Institute, Bharat Heavy Electricals Limited, Tiruchirappalli-620 014, India
ABSTRACT