US PROGRAM FOR QUALIFICATION OF EDDY CURRENT TECHNIQUES AND PERSONNEL FOR INSPECTION OF NUCLEAR STEAM GENERATOR TUBES

Mohamad Behravesh, Gary Henry*, Douglas Harris **
Electric Power Research Institute, Palo Alto, CA, USA
*EPRI NDE Center, Charlotte, NC, USA
**Anacapa Sciences Inc., Charlottesville, VA, USA