QUANTITATIVE EVALUATION OF STRAIN ENHANCED VACANCY CONCENTRATION USING NUCLEAR MAGNETIC RESONANCE PULSE TECHNIQUES IN-SITU DURING DEFORMATION OF MATERIALS

K. Linga Murty, K. Detemple*, O. Kanert* and J. Th. M. DeHosson**
N. C. State University, Box 7909, Raleigh NC 27695-7909
* University of Dortmund, 44221 Dortmund, Germany
** University of Groningen, 9747 AG Groningen, The Netherlands
ABSTRACT
start  previousOther NDT - Conference Invited Papersnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 1, pages 203 - 206