AN IMPROVED METHOD OF MAGNETIC FLUX LEAKAGE INSPECTION FOR FAR- SIDE CORROSIVE TYPE DEFECTS OF FERROMAGNETIC SPECIMENS

Kazuyoshi Sekine and Akira Iizuka
Department of Safety Engineering, Faculty of Engineering
Yokohama National University, 156 Tokiwadai, Hodogayaku, Yokohama, Japan 240
ABSTRACT
start  previousMT - Magnetic Techniquesnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 3, pages 1627 - 1630