SRC - TECHNIQUE FOR SURFACE ROUGHNESS EVALUATION AND ADJUSTMENT SENSITIVITY OF ULTRASONIC FLAW DETECTOR

V. G. Shcherbinskii
CNIITMASH, Moscow, Russia
ABSTRACT
start  previousUT - Full Paper Not Received next

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.full paper not received