APPLICATION OF NDT IN THE STEEL MAKING PLANT
Pi-Kurn Chen
China Steel Corporation, Lin Hai Industrial District T232
Hsiao Kang, Kaohsiung 81233, Taiwan, R. O. C.
Keywords: In-service testing; steel making plant, Analysis, NDT, Application
ABSTRACT To keep smooth and safe running of the steel making plant, in- service nondestructive testing in this area are to perform variety of equipments and facilities. Through administration of testing procedure standardization and personnel qualification to achieve reliability of the testing result. Equipments soundness is monitored by long term analysis of the testing results. In-service testing evaluation standards are based on the analysis of the operation condition of equipments and international NDT standards.
Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 2, pages 921 - 924