ACOUSTIC EMISSION FROM MICROFRACTURE EVENTS IN COMPOSITE PLATES

Ajit Mal and Dawei Guo
Mechanical and Aerospace Engineering Department, University of California, Los Angeles
Los Angeles, California 90095, USA
ABSTRACT
start  previousUT - Full Paper Not Received next

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.full paper not received