| SR NO | JOINT DETAILS | DESCRIPTION OF NDT |
| Penetrant Test | Radiography Test | Magnetic Particle Test | Ultrasonic Test |
| 01 | Shell longitudinal seam joints for vessel & Jacket | 100% | 100% | - | - |
| 02 | Shell to shell circumferential seam joints | 100% | 100% | - | - |
| 03 | Shell to dished end circumferential joint for vessel | 100% | 100% | - | - |
| 04 | Shell to dished end circumferential jacket | 100% | 100% | 100% | - |
| 05 | All butt joints in coil & headers. | 100% | 100% | - | - |
| 06 | Nozzle pipe to weld neck flange butt joints | 100% | 100% | - | - |
| 07 | Nozzle pipe to shell/dish joints | 100% | - | - | - |
| 08 | All fillet welds | 100% | - | - | - |
| 09 | Plate materials & flanges | - | - | - | 100% |