INCREMENTAL PERMEABILITY METHOD - ONE OPTION FOR NON-DESTRUCTIVE EVALUATION OF BOILERS TUBES

R. Grimberg, A. Savin, S. Chifan, S. Leitoiu
Institute of Technical Physics, 47 D, Mangeron Avenue, Iasi 6600, Romania
ABSTRACT
start  previousMT - Magnetic Techniquesnext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 3, pages 1643 - 1646
Publisher: Ashgate Publishing Company