ULTRASONIC DEFECTS MEASUREMENTS OF FUEL ELEMENTS WELDED JOINTS

V. T. Pronyakin, N. K. Rybakov, Yu. N. Panchenko, A. A. Bochvar*
STATE SCIENTIFIC CENTRE of Russian Federation VNIINM
*All-Russian Federal Institute of Inorganic Materials
P. O. Box 369, Moscow, 123060, Russia
ABSTRACT
start  previousUT - NDE in Nuclear Industrynext

Publication Source: Trends in NDE Science & Technology; Proceedings of the 14th World Conference on Non-Destructive Testing, New Delhi, 8-13 December 1996.Vol. 2, pages 323 - 326