744Joseph L. Rose Neural Nets For Flaw Classification Potential With Guided Waves
14W. Arnold Nonlinear Ultrasonic Phenomena - New Attempts To Improve The Reliable Detection Of The Quality Of Adhesive Bonds
36P Tscheliesnig, G. Schauritsch and G. Krenn An Acoustic Leak Detection Pig
51Chengbin Guo, Zhenyan Huang, Xiufen Wang, Xizhen Yang Structure Noise In Polycrystalline Media In Separated Transmitter Receiver Condition
191V. K. Kinra and C. Yapura and A. K. Mal* The Inverse Problem Concerning The Ultrasonic NDE Of A Layered Medium
221Prezone Karpur, Theodore E. Matikas, Robert L. Crane, S. Krishnamurthy *, Leon L. Shaw** Assessment Of Fracture Strength Of The Fiber/matrix Interfaces In Titanium-Based Metal Matrix Composites
230Vincent Garnier, Gilles Corneloup Spectral Analysis Applied To Non Destructive Testing On Concrete
250Joseph L. Rose, James Barshinger Guided Wave Applications In Aircraft Inspection
271C. H. Chen and Mr. Tzu-Hung Cheng Time-Frequency Analysis In Ultrasonic Nondestructive Testing
414V. Deutsch, P. Moller, C. Thoma* and H. Passen* New Developments Concerning Ultrasonic Testing Of Rails In Production Line
677D. E. Chimenti, O. I. Lobkis, and A. Safaeinili Exploiting Guided Waves For Materials Characterization In Plates
102William T. Clayton Innovative Ultrasonic Imaging Reactor Vessel Examination Technology For Section Xi, Appendix Viii
74V. T. Pronyakin, N. K. Rybakov, Yu. N. Panchenko, A. A. Bochvar* Ultrasonic Defects Measurements Of Fuel Elements Welded Joints
235A. Rajendran, C. Asokane, G. Elumalai and K. Swaminathan Development Of An Ultrasonic Under-Sodium Scanner For The Fast Breeder Test Reactor
443J. L. singh, Arun Kumar*, V. R. Nair, E. Ramadasan, S. Majumdar and K. C. Sahoo Quality Evaluation Of Phwr Fuel Element End Cap Weld Joints By Ultrasonic Testing Technique
444J. L. Singh, Sunil Kumar, R. Keswani, S. Muralidhar, A. K. Sengupta, H. N. Singh and K. C. Sahoo Detection Of Blister Formation And Evaluation Of Pressure Tube/calandria Tube Contact Location By Ultrasonic Velocity Ratio Measurement Technique
467P. A. Venkatachalam, J. Selva Solomon*, Agnelo Mascarenhas*, L. Pathak* and P. C. Koteswara Rao Ultrasonic Through Transmission Technique For Evaluation Of Structural Integrity Of Concrete In Nuclear Facilities
488I. Jayakumar, M. Manimohan, G. V. Chandrasekaran, S. Abdul Majeeth and P. S. Subramanyam Assuring Reliability Of Unconventional Weld Joint Configurations In Austenitic Stainless Steel Nuclear Vessels Through Non- Destructive Examination
538S. Muralidhar, S. D. Raut, R. S. Prasad, K. N. Mahule, J. K. Ghosh, V. H. Patankar*, S. R. More*, V. M. Joshi* and K. Gopalakrishnan* Development Of A C-Scan Imaging System For Detection Of Non-Bonds In Plate Type Fuel Elements
544T. R. G. Kutty**, C. Ganguly**, A. K. Bhandyopadhyay* M. D. Mangsulikar* and D. H Sastry*** Evaluation Of Elastic Constants Of Al-U And Al-U-Zr Alloys By Ultrasonic Technique
671M. S. Prakash, K. Vasudev, K. S. Lakshmi and B. Laxminarayana Monitoring Of Phwr End Cap Weld Quality By Ultrasonic Testing
57P. Revindran, M. P. R. Panicker, V. K. Ravindran, B. C. Bhaumik Ultrasonic Evaluation Of Maraging Steel Subscale Rocket Motor Chamber - An Analysis Of Associated Problem
82S. V. Rajagopal, V. P. Unnikrishnan, G. Sunilkumar, R. M. Divakaran, A. K. Rath Non-Destructive Testing Of Metallic Honeycomb Sandwich Structures For Launch Vehicle Applications
220Prasanna Karpur, Theodore E. Matikas, Robert L. Crane Advances In Ultrasonic Methods For Materials Research Of Aerospace Materials
495P. V. Sai Suryanarayana, C. Subbiah, K. Venkata Rao, K. Viswanathan and M. C. Uttam Quantitative Assessment Of Defects In M250 Maraging Steel Using Ultrasonic Testing
170Ryuichi Okuno, Yukinori Iizuka, Akio Nagamune and Katsuyuki Nishifuji New On-Line Ultrasonic Testing System Using Chirp Pulse Compression Processing
251Gautam Pasupuleti, Derrick D. Hongerholt, Joseph L. Rose and Randall M. German* Ultrasonic Sensors And Process Control In Powder Injection Molding
253Karthik Narayan, Derrick D. Hongerholt and Joseph L. Rose Ultrasonic NDE Of Pressed Metal Parts
454S. Venkadesan, P. Palanichamy, M. Vasudevan and Baldev Raj Ultrasonic Velocity Measurements - A Potential Sensor For Intelligent Processing Of Austenitic Stainless Steels
564Klaus Berner, Holger Stilke, Gerda Bach* and Horst Ballmann* Fully Automatic Ultrasonic Testing Plant For Online Inspection Of Heavy Plate With Plate Thicknesses Upto 150 Mm Including Inspection For Surface Defects In Plate Head And Tail Regions
605M. Kroning*, H. J. Salzburger*, Y. Smorodinski**, V. I. Mironenko*** Measurement Of Wall-Thickness At Extreme Temperatures Using Emats
606Surendra Singh Emerging Ultrasonic Techniques For Process Sensing And Control In Manufacturing
650Krishnan Balasubramaniam Ultrasonic Monitoring Of The Pultrusion Manufacturing Process
537J. K. Ghosh, S. Muralidhar, S. D. Raut, S. Rajendran*, G. Singh*, D. Venkatesh*, P. K. Bhaumik* and M. S. Ramakumar Development Of An Ultrasonic Inspection Gig For Monitoring A Buried Pipeline
628M. Thavasimuthu, A. Joseph, A. S. Ramesh, C. V. Subramanian, T. Jayakumar and P. Kalyanasundarm Assessment Of In Service Degradation Of Conical Inlet Of A Waste Boiler In A Chemical Plant By NDT Methods
15D. Dutta Development Of Rotary Probe Ultrasonic Testing System Of Large Diameter Seamless Pipes For Oil And Gas Industries In India
19Zheng Kaisheng and Chen Yucheng, Baoji Non-ferrous Metals Works A New Ultrasonic Testing Technique For Titanium Bars With Small Diameter
135Yudhisther Kumar, Ashok Kumar and Basant Kumar Non-Destructive Evaluation Of Rods By Ultrasonic C-Scan System
660Peng Yingqiu, Zhu Jianguo, Li Jien A New Ultrasonic Testing Technique No Dead Zone For Small Bars With Coarse Gain Structure Development On Line Focussed Creep Wave Probe
672G. S. S. Sastry N. R. Rao J. Shankar Kumar Evaluation Of Circular Bar For Critical Applications Using NDT Techniques
31Junji Takatsubo, Shigeyuki Yamamoto, Akira Watanabe* and Kazuhiro Kametani* Ultrasonic Technique For Quantitative Evaluation Of Dispersed Particles In Metal Matrix Composite
32J. Prasad NDE For Carbon-Fibre-Composites Through Ultrasonics: Indian Experience
35Shao Zebo, Wang Xiaoling and Song Shubo Ultrasonic Inspection Of The Impact Damage To Cerp Laminated Plate
81Hyunjo Jeong*, David K. Hsu** and Peter K. Liaw*** Determining The Constituent Volume Fractions Of Metal Matrix Composites By A Multiple NDT Technique
117Hans Erik Gundtoft and Kaj Kvisgaard Borum Evaluation Of Advanced Fibre Composite And Sandwich Structures By Ultrasonic Examination
233Pravesh Kumar and Ravi Prakash Mechanical Engineering Group Quality Assessment Of Glass Fibre Composites By Acousto Ultrasonic Technique
298Kiyoshi Ishihara*, Osami Kobori**, Isamu Sakamoto**, Masayuki Sato***, and Masaru Omura**** Ultrasonic Measurement Of Development Of Elastic Anisotropy Due To The Applied Strain In Fiber Reinforced Plastics
387H. N. Sudheendra, M. R. Madhava, M. Subba Rao and B. R. Somashekar Ultrasonic Through Transmission Inspection Of Co-Cured Cfrp Aircraft Components
391M. V. Hosur and C. R. L. Murthy Ultrasonic Evaluation Of Delamination In Quasi-Isotropic Cfrp Laminates Subjected To Low-Velocity Impact
418Basant K. Parida and D. R. Sankhala* Structural Damage Assessment Of Cfc-Components Through Ultrasonic NDE Method
626D. Ponraju*, Letha Sebestian*, S. Viswanathan*, A. Natarajan*, P Palanichamy**, T Jayakumar** and Baldev Raj** On-Line Measurement Of Residual Monomer During Polymerization Of Acrylamide Using Ultrasonics
649Krishnan Balasubramaniam, Nain S. Rao and Yuyin Ji Characterization Of Material Properties Of Multi-Layered Fiber Reinforced Composite Structures Using Inverse Ultrasonic Methods
10V. K. Srivastava and Pravesh Kumar* Behaviour Of Modified Acousto-Ultrasonic In Gfrp Composites
33Gouri S. Bhuyan NDE Based Grading And Quality Assurance Of New And Old Utility Wood Poles
169Aamir Khalid, Victor Kearley** The Development Of Ultrasonic Non-Destructive Evaluation Techniques For The In-Situ Inspection Of Wooden Transmission Poles
194T. L. Shaji, S. Somayaji* and M. S. Mathews** Evaluation Of Structural Timber In Historic Buildings Using NDT Techniques
238K. Shyamasundar, B. S. Aswathanarayana and M. Venugopal Naidu Grading Of Swan Timber - Elasto Sonic Way
301Vasundhara Non-Destructive Field Testing Of The Behaviour Of Yielding Cable Bolts With Mini Cages
408Narayan R. Joshi Ultrasonic Interference Spectroscopy For Plastic Ic Packages
416K. S. Tan, P. Hing**, B. S. Wong* and S. C. Ong* Ultrasonic C-Scan Of Embedded Foreign Inclusions In Sintered Ceramics
422M. V. M. S. Rao, D. S. N. Murthy, G. M. Nagaraja Rao*, K. Shivakumar* and S. Udayakumar* Estimation Of Crack Density Of Heat-Soaked Granite Using Ultrasonics
485G. M. Nagaraja Rao, C. R. L. Murthy* and N. M. Raju Study Of Effect Of Strain Rate On Critical Damage In Granite By Ultrasonic Imaging
490Manish Gupta, Hasan Abdullah and A. K. Dhawan Application Of Laboratory Non-Destructive Techniques For Rocks
526S. Kamle, S. Upreti*, N. G. R. Iyengar and A. Kumar* NDT Of Adhesive Joints Using Transverse Waves
534A. K. Mukhopadhyay, D. Basu, S. Mukherjee and K. K. Phani Ultrasonic Velocity Measurement For Characterisation Of Porosity In Sintered Ceramics And Metals
676V. Rajendran*, H. A. El. Batal** and F. A. Khalifa** Compositional Dependence Of Acoustic Properties And Structural Role Of Lead In Lead Silicate Glasses
224T. T. Wu and J. S. Fang Application Of Transient Elastic Waves To The Nondestructive Evaluation Of Concrete
225Chung-Yue Wang* and Y. F. Chang** Evaluation Of The Bonding Condition Between Steel Plate Patch &Amp; Strengthened Concrete Structure
241Lin Weizheng Yuan Yiyong Ultrasonic Detection Of Cement Concrete Pavement Thickness
489Chih-Hung Chiang and Cho-Liang Tsai The Nondestructive Evaluation Of Coated Steel Bar In Reinforced Concrete Structure
571Mohamad Pauzi Ismail, Kamarudin Mohd. Yusof* and Abdul Nassir Ibrahim Ultrasonic Relative Amplitude Method For Predicting The Strength Of Concrete
86Yu. V. Lange, S. I. Voropaev, Moujitski, S. Hubbard* New Means For Nondestructive Testing Of Multi Layer Structures Of Composites
337Yan-Rongming, Deng-Jianping* The Smallest Defect That Can Be Detected Using Ultrasonic Testing
399Ashok J. Trivedi and Rajul R. Parikh Ultrasonic Inspection Of Shell Body Using Multi Channel Ultrasonic Immersion Testing System
460J. Verkooijen and N. Trimborn Practical Experiences In The Application Of Advanced Ultrasonic Equipment To Decrease Downtime Through Non Intrusive, True Condition Assessment
476R. Prasad and S. Kumar* Study Of Correlation Between Ultrasonic Flaw Indications And Types Of Defects
561R. Ambardar, T. Jayakumar*, S. K. Pathak and O. Prabhakar Effect Of Surface Roughness On Ultrasonic Echo Amplitude In Aluminium-Copper Alloy Castings
579C. V. Subramanian, A. Joseph, A. S. Ramesh, T. Jayakumar, P. Kalyanasundaram and Baldev Raj Wall Thickness Measurements Of Tubes By Internal Rotary Inspection System (Iris) - A Comparative Study With Metallography
607Dong-Man Suh and Whan W. Kim* A New Ultrasonic Technique For The Detection And Sizing Of Small Cracks In Stud Bolt Threads
683Jelena vojvodi Gvardjancic *, Joze Zorko** Size Estimation Of Reflector By Ultrasonic Inspection
669Ashok Tiwari and C. B. Shah Evaluation Of Distressed Structures Using NDT Techniques- A Few Case Studies In Gujarat
708V. K. Rajan Condition Monitoring And Life Assessment Of Diesel Engine Through Non-Destructive Testing
580Saju Skaria and C. R. L. Murphy Non-Destructive Evaluation Of Advanced Composite Honeycomb Structure - Some Studies
630C. V. Subramanian, M. Thavasimuthu, A. S. Ramesh, T. Jayakumar and P. Kalyanasundaram Fatigue Crack Growth Studies On A "Tee Junction" Using Ultrasonic Non-Destructive Methods
642V. R. Singh Diagnosis Of Bone Fractures By Using An Acoustic Technique
4P. Prokhorenko, N. Gil, G. Konovalov and A. Mayorov The Testing Of The Perpendicular To The Free Surface Adhesion Boundary
247Myoung-Seon Choi and Young-Sang Joo Resonance Scattering Of Acoustic Waves From A Nuclear Fuel Rod In Water
195S. Devolder, M. Wevers, P. De Meester, O. Leroy*, *K. U. Leuven Campus Kortrijk Material Research Using The Accousto-Optic Technique
586Hirunobu Yuki, Haruo Ishikawa and Yasuji Wakiyama Fractal Characteristics Of Delamination In Cfrp Laminates
608Kaj Kvisgaard Borum and Hans Erik Gundtoft A New Documentation System As Part Of Quality Assurance In Non- Destructive Testing
20Zheng Kaisheng, Liu Jingzhong, Chen Yucheng A Technique Of Ultrasonic Testing For No Upside-Dead Zone - The Universal Ultrasonic Probe For No Upside-Dead Zone
59M. C. M. Bakker Directivity Of Probes In NDE-Inspection
60Elfgard Kuhnicke, U. Volz Designing Ultrasonic Transducers For Layered Media By Means Of Green'S Functions - A Calculation Software
66Yougen Peng An Acoustic-Testing Sensor Based On Acousto-Magnetic Effect
103Katsuyoshi Kimura, Mamoru Yamoto* Dgs Diagrams For Point Focusing Ultrasonic Normal Probes
149Chen Yifang, Zhang Jiajun An Ultrasonic Transducer To Test The Connecting Quality Of Double- Chilled Roller
156D. Desruelles - O. Burat - G. Pierre Ultrasonic Phased Array Probes For High Speed Inspection Of Tubes
175Song Shaohe, Wu Kai A New Ultrasonic Wave Probe Used In Detecting Turbine Blade'S Roots
256Bruce Drinkwater And Peter Cawley The Practical Application Of Solid Coupled Ultrasonic Transducers
310Daniel De Vadder, Alain Lhèmery* Improved Resolutions With Non-Uniform Ultrasonic Transducers Old Ideas, New Realizations
362Reyes and C. Gonz et. al Design And Implementation Of Linear And Point Focused Transducers For Non-Destructive Testing
506V. N. Bindal, S. K. Jain, P. S. Krishna Mohan Rao*, M. V. B. Rao and Subhash Chandra Design Considerations Of Low Frequency Transducers For The NDT Testing Of Concrete, Timber And Like Materials
558P. Blanquet, T. Demol and C. Delebarre Application Of Array Transducers To Health Monitoring Of Aeronautic Structures
691D. A. Hutchins*, A. G. Bashford*, W. M. D. Wright*, D. W. Schindel**, and A. Kumar*** Air-Coupled Ultrasonic Capacitance Transducers For NDT
41G. L. Workman and J. Walker Update On The Development Of A Robotic Acousto-Ultrasonic System
116S. R. More, V. H. Patankar, V. M. Joshi, K. R. Gopalakrishnan An Advanced Ultrasonic Imaging System For NDT/NDE
185H. V. Singh and D. V. K. Charan Automatic Ultrasonic Scanning
215Sung-Jin Song, Hak-Joon Kim and Won-Suk Sung Development Of An Intelligent Ultrasonic Evaluation System With A Multi-Axis Portable Scanner
217Wang Zhengxian Zhang Zenggen The Application Of Lcd In Computerized Ultrasonic Flaw Detector
328B. Nouailhas, A. Schumm Coupling Cad And Ultrasound
357Motoharu Goto Applications Of Portable Phased Array Ut System
686William Paul Motzer Ultrasonic B-Scan System Used To Inspect Composite Airplane Parts
39Hung-Fa Shyu*'**, M. W. B. Lock* Ultrasonic Testing System With Split Spectrum Processing For Haz Creep Damage Evaluation
69Alexander M. Akhmetshin High-Sensitive Ultrasonic Deep Probing Of Low-Contrast Structures With Unknown Law Of Receiver Signals Distortion By Means The Generalized Matched-Filtering Method
172Yoshinori Fukuda and Hajime Kitagawa Classification Of Ultrasonic Flaw Signals By Means Of Time-Frequency Analysis
211Zhu Senyuan, Pen Xianchu*, Wang Xuhui**, and Tang Chenghui** Distinguish The Echo Of Signal Of Transverse Wave And Longitudinal Wave In Ultrasonic Testing By Computer
635C. Rajagopalan, P. Kalyanasundaram and Baldev Raj Uncertainty Management In Knowledge Based Systems For Nondestructive Testing - An Example From Ultrasonic Testing
658P. Barat*, P. Mukherjee*, and Debashree Dutta** Fractal Characterization Of Back Scattered Ultrasonic Signals
145D. Datta, N. N. Kishore*, P. Munshi* Features Of Ultrasonic NDT To Identify Defects In Composite Materials Modelled By Fem
214J. Murai, T. Ida and T. Shiraiwa Acoustic Field Of Spherical Focusing Transducer (Ii)
227J. F. Chai* and T. T. Wu** Measurement Of Surface Wave Velocities In A Prestressed Anisotropic Crystal And Its Application To Nondestructive Testing
276P. P. Delsanto, E. Ruffino, V. A. M. Luprano*, G. Montagna *, V. I. Anisimkin ** Parallel Processing Simulation Of The Propagation Of Baw-Saw Transducer Generated Waves
277P. P. Delsanto, R. B. Mignogna*, V. Chiroiu**, L. Monteanu** Modeling Interfaces: Analytical And Numerical Techniques
339Yan-Rongming*, Zhou-Guangping and Qiu-Wenbin A New Method To Enhance The Resolution Of Ultrasonic Testing
609H. Tavossi and B. R. Tittmann Ultrasonic Characterization Of Sediment Model Media
42D. Devaraj, K. G. Prabhakaran* and P. S. Subramanyam Effect Of Microstructure And Weld Geometry On The Ultrasonic Evaluation Of Thick Dissimilar Metal Weld
113Zheng Zhongxing, Hu Shaohai, Teng Yongping, Cui Jiangying, Qiu Ruichang The Study Of Ultrasonic Imaging System For Austenitic Welds
201Chen Qinglin A New Focusing Probe Of Ultrasonic And Its Application In Testing Welds
456S. Mohan, S. Ravishankar, N. Masilamani, V. N. Misale and S. C. Durgad Ultrasonic Immersion Testing Of Weldments
466P. Annamalaisamy, T. V. Subash, K. C. Chandran, S. Abudl Majeeth and P. S. Subrahmanyam Investigation Of Spurious Ultrasonic Indication In A Critical Circumferential Butt Joint - A Case Study
469M. Bandyopadhyay, P. P. Nanekar, B. K. Shah, R. Ramanathan, M. D. Mangsulikar and P. G. Kulkarni Ultrasonic Characterisation Of Intergranular Stress Corrosion Cracking In Austenitic Stainless Steel Welds
512M. Palaniappan, R. Subbaratnam, A. Baskaran and R. Chandramohan Effect Of Repeated Repairs On The Austenitic Stainless Steel Welds Upon The Ultrasonic Examination Sensitivity
513R. Subbaratnam, M. Palaniappan and A. Baskaran Ultrasonic Examination Of Heavy Austenitic Stainless Steel Welds - Our Experience
679Troitskii V. A Nondestructive Testing Of Multilayer Welded Structures
165Bryan Bridge and Kuroush Merrikh Ultrasonic Backscatter Measurements Of Grain Size Variations Illustrated By Studies On Heat Treated Chrome-Nickel Stainless Steel
274Takuichi Imanaka, Yoshikazu Yokono, Shigeyuki Matsubara, Kazuhiro Mukai

*Yukimitsu Okano, *Yasuo Kurozumi, *Yasuhiro Kawaguchi

Nondestructive Evaluation Of Materials Degradation In Power Plants -Detection Of Thermal Embrittlement And Igscc
275V. Krishnamurthy, G. Venkataraman and R. S. Babu Evaluation Of Ultrasonic Test Indications Of Creep Damages In High Temperature Pressure Parts Of Power Plants
459N. Trimborn and J. Verkooijen Hot Hydrogen Attack: A Novel Approach For Reliable Detection And Monitoring
468B. K. Shah, P. P. Nanekar, M. Bandyopadhyay, A. K. Bandyopadhyay, A. R. Biswas and P. G. Kulkarni Ultrasonic Characterisation Of Ageing Degradation During Long- Term High Temperature Exposure In Nickel-Base Alloy 625
481Vaidehi Ganesan, P. Palanichamy, C. Rajagopal, P. Kalyanasundaram and Baldev Raj Ultrasonic Characterisation Of 748 K Embrittlement In 12%Cr- Ferritic Steel
522Manish Gupta, Hasan Abdullah and A. K. Dhawan Application Of Laboratory Non-Destructive Techniques For Rocks
545J. C. Pandey, R. Jha, M. P. Singh* and O. N. Mohanty Ultrasonic Attenuation Technique And Quality Of Steel Products
629P. Palanichamy and Jayakumar Grain Size Measurements By Ultrasonic Rayleigh Surface Waves
94Marie-Helene Nadal, Cyril Hermerel, Christian Gondard and Luc Paradis Determination Of Elastic Constants In A Materials Submitted To High Temperatures With An Ultrasonic Method
134Ashok Kumar, Yudhisther Kumar and Basant Kumar A New Approach Of Ultrasonic Attenuation Measurement For NDE And Material Characterization
148Chen Yifang, Zhang Jiajun A Research On Testing Elastic Moduli Of Workpiece Materials
219Theodore E. Matikas, Prasanna Karpur, Robert L. Crane, S. Shamasunder* Correlation Of Various Elastic Moduli With Relative Density Of Porous Alpha-Two Titanium Aluminide Compacts
236N. K. Batra, K. E. Simmonds and R. B. Mignogna Determination Of Elastic Constants Of Anisotropic Materials From Propagation Of Ultrasonic Waves Along Arbitrary Symmetry Directions
351Jose P. Panakkal Longitudinal Ultrasonic Velocity As A Predictor Of Material Properties Of Porous Materials
415K. S. Tan and P. Hing* On The Elastic Modulus Of Alumina-Zirconia Composite Using Ultrasonic Through Transmission
80K. S. Tan, N. Guo* and B. S. Wong* Evaluation Of Near Surface Delaminations In Laminate Plates Using The Lamb Wave Amplitude Technique
252Semyen P. Pelts, Dale Jiao and Joseph L. Rose Transducer Influence On Lamb Wave Excitation In Composite Plate
254Hyeon Jae Shin, Robert Yi and Joseph L. Rose Defect Detection And Characterization In Power Plant Tubing Using Ultrasonic Guided Waves
257David N. Alleyne, Alan M. Lank*, Peter J. Mudge* and Peter Cawley The Lamb Wave Inspection Of Chemical Plant Pipework
557T. Demol, P. Blanquet and C. Delebarre Optimization Of Linear Array Transducers For Lamb Waves Generation
92Frederique Tardy, Marie-Helene Nadal, Christian Gondard, Luc Paradis, Jean-Claude Baboux Local Characerization Of Materials Using An Impulse-S. A. M. Technique In The 10 Mhz-20 Mhz Range
128Ute Bergmann*, F. Bergner**, K. J. Langenberg***, Ch. Hofmann*** Ultrasonic Time-Of-Flight Diffraction Method For Monitoring Stable Crack Growth
137F. H. Dijkstra and J. A. de Raad Tofd &Amp; Acceptance Criteria: A Perfect Team
147D. Datta N. N. Kishore*, P. Munshi* Application Of Acoustic Tomography In Nondestructive Testing
367S. Ramnath, Agnelo Mascarenhas, J. Selva Solomon and L. Pathak Simplified Instrumentation For Pc-Based Saft Systems
413C. A. Lamy, J. M. A. Rebello** and J. Charlier* Sizing Of Inclined Surface Flaw By The Time-Of-Flight Technique
458K. S. Venkataraman and A. Mclay* The Performance Of The Time-Of-Flight Diffraction (Tofd) Technique In Various International Round-Robin Trials And The Continuing Research Work Underway Today
273Byoung-Geuk Kim and Sekyung Lee, and Teruo Kishi* Newly Designed Acoustic Lens For Point-Focusing Of Surface Waves: Use Of Conventional Ultrasonic Transducer
263Branislav Sladojevic Ultrasonic Testing Of Heavy Forgings
430Ju Ximin The Computer-Controlled Automatic Ultrasonic Flaw Detection System For Thin Wall Tubular Product
721P. M. Deshpande, V. V. Gokhale, Rita D. Abbi, and C. M. Sinha Estimate Of Concrete Strength By Ultrasonic Velocity
722Martin Kuna*, Josef Plasek*, Hank Bakker**, and Jan H. Kooi** Verification Of Possibilities For The Check Up Of Undercladding Cracks And Application Of Tofd Method For The Inspection Of Materials With Cladding
17Yu Fengnian The Nondestructive Testing Of The Quality Of Hard Alloy Products
21Zhang Junzhe High Resolution Ultrasonic C-Scan Detecting For The Electron Beam Welding Of Ring Samples
46V. G. Shcherbinskii Src - Technique For Surface Roughness Evaluation And Adjustment Sensitivity Of Ultrasonic Flaw Detector
49Teng Yongping Numerical Investigation Of A Wideband Ultrasonic Focusing Transducer
65V. Fedorov; Y. Gordeev, V. Letunovsky, S. Teremov Non-Destructive Methods Of Control As A Means For Quality Testing And Sintered Powder Composites Construction
71Yanis I. Bulbik*, Nicolaj V. Vasilenko*, Lev N. Loginov** Nondestructive Evaluation Of Defects In Not-Pressed Ceramic Nozzles By Combined Electroacoustic Technique
83Kyoji HOMMA and Toshi MIYASHITA Application Of Neural Network To Ultrasonic Flaw Detection In Layered Media
84V. Konnov, V. Timoshenko Strategy Of Methods And Means Development For Nondestructive Inspection Of Reusable Aerospace Vehicles Thermal Protection
87Dr. Albrecht Maurer and Paul Schneider An Advanced Ultrasonic Test Electronics For Flexible Use In Systems' Applications
138L. M. Gelman, Y. V. Burau, V. I. Krytsyn Optimization Of Signal Processing For Acoustic NDT
154Sandor Popovics et al The Ultrasonic Pulse Velocity Test As Specified By Various Standards
163Steen Arnfred Nielsen, Hans Erik Gundtoft and Kaj Kvisgaard Borum Ultrasonic Fan-Beam Measurements For Tomographical Image Reconstruction Of Composite Materials
171Dawei Guo and Ajit Mal Lamb Waves From Microfractures In Composite Plates
197I N Prassianakis The Study Of Materials Elastic Properties Dependence On The Frequency And Temperature, Using Ultrasounds
210Zhu Jinying, Chen Longzhu Finite Element Studies Of Ultrasonic Pulses In Concrete
282Anurag P. Mairal, Leonard J. Bond*, Alan R. Greenberg*, and William B. Krantz Development And Application Of Acoustic Time-Domain Reflectometry For Real-Time, Noninvasive Characterization Of Membrane Fouling In Reverse Osmosis (Ro) Desalination
287G. J. Molina and Y. M. Haddad On The Characterization Of Impact Properties Of Engineering Materials Using Acousto-Ultrasonics - A Pattern Recognition Approach
302Liu Zhenqing, Liang Sui*, LuMingda**, Wei Moan* The Artificial Neural Network Adaptive Filter For The Ultrasonic Nondestructive Testing Signals Of Coarse Grained Materials
330Y. Shen, C. Ozzano, N. Pietranera, F. Rosatelli, E. Bellafronte*, M. Portesine* High Frequency Ultrasonic Evaluation Of Power Semiconductor Devices
336L. V. Voronkova, Cem, V. A. Voronkov Flaw And Structure Detection Of Cast Iron Foundings By Means Of Surface And Head Ultrasonic Waves
338Yan-Rongming, Li-Hai Quan* The Sound Field And Focusing Laws Of Spherical Lens For Ultrasonic Testing
343P. Calmon, A. Lhémery, I. Lecoeur-Taïbi Modeling Tools For Ultrasonic Inspection
344Ph. Benosîst, M. Talvard, P. Calmon, M. Serre Research And Development At The Cea For NDT In The Nuclear Industry
348Udaya B. Halabe, Samer H. Petro, Hota V. S. GangaRao NDE Of Wooden Structural Members Using Ultrasonic Technique
350G. S. Bhuyan, E Sperling*, J. Bowker** and G. Rousseau** Effectiveness Of Non-Destructive Evaluation Techniques For Sizing Defects Found In Petro-Chemical Pressure Vessels
360Dawei Guo and Ajit Mal Lamb Waves From Microfractures In Composite Plates
401Dr. C. R. L. Murthy, Thomas C. Koshy* Characterization Of Delaminated Zones In Ablative Composites By Acoustic Microscopy
403S. N. Chakravarty, D. K. Bhattacharya* and A. K. Mandal Grain Size Control In Cr-Mn Steel Pins By Ultrasonic Attenuation Technique
440S. Muralidhar, S. Gangotra, R. Keswani, S. D. Raut, P. K. Ouseph, J. K. Ghosh and K. C. Sahoo Ultrasonic Characterisation Of Zirconium Hydride Blisters
445J. L. Singh, A. B. Tamhana, H. N. Singh and K. C. Sahoo Ultrasonic Flaw Evaluation Of Reactor Operated Pressure Tubes
462Surendranath Singh Emerging Ultrasonic Techniques For Process Sensing And Control In Manufacturing
483P. P. Kumaraguru and L. Lahiri Non-Destructive Evaluation Of Rubber/cfrp Hybrid Ablative-Linear By Pulse Ultrasonic Spectroscopy, Swept Frequency Ultrasonics And Low Frequency Vibration Analysis Techniques
497Petre Petculescu The Analysis Of The Focal Region Of Focused Ultrasonic Beams
500Jens Petter Tronskar, Chow Ngai Mun and Pradip Goswami Condition Monitoring And Engineering Critical Assessment Of In-Service Pressure Vessels By Advanced Non-Destructive Examination Method
501Kwo-Chen Hou, Chi-Min Chang, Hong-Yie Chen & Chih-Han Wang Ultrasonic Techniques For Inspecting The Adhesive Quality Of Rocket Motor Nozzles
514Ajit Mal and Jyj-Herng Shih Nondestructive Characterization Of Stiffness Degradation In A Titanium Matrix Composite During Fatigue Loading
519Nripendra Kumar and A. K. Dhawan Importance And Techniques Of Non-Destructive Testing For Rock Mechanics Investigations
524S. S. Iyer and R. S. Vaghasiya Geometric Computer Plots Of Focussed Ultrasonic Beams Crossing Interfaces
527L. M. Tolani, V. K. Seth and A. K. Shrivastava Design And NDT Of Critical Weld Joint
549Ajit Mal and Dawei Guo Acoustic Emission From Microfracture Events In Composite Plates
603B. Suri, N. Chandrasekaran, G. K. Vijh, A. K. Sthapak Non-Destructive Testing Of Concrete And Masonry Dams Using Ultrasonic Pulse Velocity Technique: Case Histories
611V. N. BINDAL*, S. K. JAIN, A. D. PRASAD**, & REETA GUPTA* Studies On A Cylindrically Focused Probe For The Ultrasonic NDT Applications
637Ju-Ginglong and Lei-Zhengge Ultrasonic Mode Transformation For Inspecting Round Wire Compression Springs
640D M Findeis and J. Cryzagoridis Detection Of Unwanted Liquids In Sealed Gas Bottles
647S. Viswanath*, R. M. V. G. K. Rao** and C. R. L. Murthy*** Ultrasonic Imaging Of Defects And Damage In Carbon Reinforced Fiber Plastic Components
664A. N. GUZ' On Foundation Of Non-Destructive Ultrasonic Method Of Determination Of Two-Axial Initial (Residual) Stresses
666Rainer Frielinghaus Ultrasonic Testing Of Spot Welds In The Car Industry
678Prof. V. A. Troitskii, A. N. Kozin New Technological Capabilities Of Ultrasonic Testing Of The Vver-Type Reactor Metal
680V. A. Troitskii, I. Ya. Shevchenko, V. F. Baldakov Automated Ultrasonic Testing Of Pipeline Welded Joints
693M. N. Saraf, R. K. Gupta, K. M. Chaudhary and G. N. Mathur Estimation Of Flaws In Impacted Frp Composites By Ultrasonic Flaw Detector
706Joseph L. Rose, Dale Jiao*, and Jack Spanner, Jr.** Ultrasonic Guided Wave NDE For Piping
728Dr. Hansgeong Thiele The UT-MIPA-Weldscanner-A New Approach In The Inspection Of Pipeline Girth Welds
UT - Laser
262Detlef Mampel and Asoke K Nandi Comparative Study Of Deconvolution Algorithms
651Krishnan Balasubramaniam, Vimal Vinod Shah and Daniel Costley Laser Generated Guided Ultrasonic Wave Applications In Non- Destructive Evaluation
694P. K. Raju*, and A. Gerad** Anisotropic Damage Evolution In Brittle-Brittle Composites Under Uniaxial Tension And Their Ultrasonic Measurement
568Ching-Chung Yin and Lo-Cheng Shieh Characterization Of Filament Wound Composite Hollow Cylinders By Laser-Induced Ultrasound