The Experimental and Theoretical Study of Optima Shape at Plugs for Jointing Elements in Wood-based Materials
Szava, Ioan; Curtu, Ioan; Ciofoaia, Vasile;Botis, Marius ; Dogaru, Florin Transilvania University of Brasov, Romania, Ro 2200 Brasov; Bul. Eroilor nr.29.
ABSTRACT
The usual shape of plugs at gluing zone is circular section, but at present there is attempts to use plugs with square and hexagonal section, too. These solutions assure possibility to introduce more adhesive, thus increase the strength of joints. With an original holographic stand the authors makes some detailed researches for establishing the optima shape of the plug section. Thus, was established the condition for a maximal angular stiffness of the joints: d+(1.2) mm > D.
Publication Source: Proceedings of the 12th International Symposium on Nondestructive Testing of Wood University of Western Hungary, Sopron, 13-15 September 2000, ISBN 963 7180 88 5 Publisher: University of Western Hungary, H 9400 Sopron, P.O.Box 132, FAX: +36 99 311 103