FIGURE 3. |
| Legend | ||
| Site# | AFT | FWD |
| 1 | 0.070 | 0.020 |
| 2 | 0.090 | 0.030 |
| 3 | 0.080 | 0.130 |
| 4 | No Crack | |
| 5 | 0.065 | 0.080 CNB* |
| 6 | 0.115 | 0.080 |
| 7 | 0.020 | 0.065 CNB |
| 8 | 0.065 CNT | 0.075 CNT |
| 9 | 0.045 CNT | 0.040 |
| 10 | No Crack | |
| 11 | 0.040 | 0.075 |
| 12 | 0.020 CNB | 0.135 |
| 13 | 0.125 | 0.040 CNT |
| 14 | 0.040 CNB | 0.095 |
|
*CN= Corner Notch B= Bottom of 2nd Layer T= Top of 2ndLayer | ||
| |NDTnet| |