Topics
|
|
|
We.1.7.1
|
Real time in-situ monitoring of metallurgical phenomena with laser ultrasonics
Meilland, P., ARCELOR Research, Maisières-lès-Metz (France) Damoiselet, F., ARCELOR Research, Maisières-lès-Metz (France) Nogues, M., ARCELOR Research, Maisières-lès-Metz (France) Midroit, F., ASCOMETAL CREAS, Hagondange (France)
|
Manuscript
|
|
We.1.7.2
|
ACOUSTIC EMISSION AND ULTRASONIC INSPECTION FOR THE MONITORING OF CURE RELATED DEFECTS IN THICK RTM PRODUCTS
Heida, J.H., National Aerospace Laboratory NLR, Amsterdam (The Netherlands) Hart, W., National Aerospace Laboratory NLR, Amsterdam (The Netherlands)
|
Manuscript
|
|
We.1.7.3
|
Ultrasonic Sensor Tool for Automated Material Inspection in Milling Machines
Schmitt, R., RWTH Aachen
(Germany)
Hafner, P., RWTH Aachen
(Germany)
|
Manuscript
|
|
We.1.7.4
|
Fully-Connected Remote Visual Inspection (RVI)
Pellegrino, B., GE Inspection Technologies, Flanders (USA) Clark, S.R., GE Inspection Technologies, Flanders (USA)
|
Manuscript
|
|
We.1.7.5
|
EDDY CURRENT INSPECTION TO MEASURE THE DISTRIBUTION OF SILICIUM IN ALUMINUM MOTOR UNITS
Junger, M., Rohmann, Frankenthal
(Germany)
Lindecke, L., Rohmann, Caputh
(Germany)
|
without manuscript
|
|
Th.3.7.1
|
Micromagnetic testing for rolled steel
Wolter, B., Fraunhofer IZFP, Saarbrücken
(Germany)
Dobmann, G., Fraunhofer IZFP, Saarbrücken
(Germany)
|
Manuscript
|
|
Th.3.7.2
|
QUANTITATIVE NON-CONTACT ULTRASOUND TESTING AND ANALYSIS OF MATERIALS FOR PROCESS AND QUALITY CONTROL
Bhardwaj, M., The Ultran Group, State College PA (USA) Eischeid, T., The Ultran Group, State College PA (USA) Vun, R.Y., The Ultran Group, State College PA (USA)
|
Manuscript
|
|
Th.3.7.4
|
In-line ultrasonic automatic inspection of steel bar products
Garcia Ares, E., INTERLAB IEC, Madrid (Spain) Alejandro, M.P., INTERLAB IEC, Madrid (Spain) Blanco, C., INTERLAB IEC, Madrid (Spain) Garcia Alonso, J.L., INTERLAB IEC, Madrid (Spain)
|
without manuscript
|
|
Th.3.7.5
|
THE PLAN FOR PULSE MAGNETIC ON-LINE TESTING OF MECHANICAL PROPERTIES OF ROLLED PRODUCTS
Matyuk, V., National Academy of Science of Belarus, Institute of Applied Physics, Minsk (Belarus) Hartmann, H., Forschungs- und Qualitätszentrum Brandenburg, Eisenhüttenstadt
(Germany)
Reichelt, H., Forschungs- und Qualitätszentrum Brandenburg, Eisenhüttenstadt
(Germany)
Schmidt, R., Forschungs- und Qualitätszentrum Brandenburg, Eisenhüttenstadt
(Germany)
Delendick, M., National Academy of Science of Belarus, Institute of Applied Physics, Minsk (Belarus) Osipov, A., National Academy of Science of Belarus, Institute of Applied Physics, Minsk (Belarus) Pinchukov, D., National Academy of Science of Belarus, Institute of Applied Physics, Minsk (Belarus)
|
Manuscript
|
|